Fourth Firing (Mar's Landers'), Page 4
Jan 28, 2004 (12:01 am) - Feb 2, 2004 (7:30 pm)


door sealed Using slip to seal the major cracks in the door. I decided to seal loosely - the slip sort of crackles as it dries. Furutani would sometimes quick cool his kilns for 1 to 1.5 hours. I'm not so brave yet, but a loose seal makes me feel a little wild at least.